THREAD: AS8879
MATERIAL:
  • 3AL - 2.5V Titanium alloy per AMS6940 (UNS R56320).
HEAT TREAT: Per AMS - H - 81200.
FINISH:
  • Coat outside of nut (ID & C'Bore optional) with dry film lubricant coat per AS5272, Type I, plus (optional) cetyl alcohol lubricant.
PERFORMANCE: 23MI44
1 - 5 of 5 | Results Per Page | View | Unit of Measure
1 

Item #

A

B

C

D

L - MAX

M - MAX

Axial Tensile Strength lbf Min

Thread per AS8879

EN1181ND-5 N/A 0.288-0.294 in N/A 0.167-0.173 in N/A 0.247 in N/A 0.219 in N/A 0.275 in N/A 0.219 in N/A 1940.000 lb N/A 0.1640-32 UNJC-3B
EN1181ND-6 N/A 0.318-0.324 in N/A 0.206-0.212 in N/A 0.275 in N/A 0.242 in N/A 0.295 in N/A 0.242 in N/A 2500.000 lb N/A 0.1900-32 UNJF-3B
EN1181ND-8 N/A 0.418-0.424 in N/A 0.268-0.274 in N/A 0.359 in N/A 0.323 in N/A 0.340 in N/A 0.323 in N/A 4300.000 lb N/A 0.2500-28 UNJF-3B
EN1181ND-10 N/A 0.532-0.542 in N/A 0.330-0.338 in N/A 0.435 in N/A 0.390 in N/A 0.435 in N/A 0.390 in N/A 6300.000 lb N/A 0.3125-24 UNJF-3B
EN1181ND-12 N/A 0.642-0.652 in N/A 0.392-0.400 in N/A 0.534 in N/A 0.483 in N/A 0.475 in N/A 0.483 in N/A 8700.000 lb N/A 0.3750-24 UNJF-3B